[Chiny]PS Plate

Thickness: 0.15-0.30mm Spectral Sensitivity: 3000W iodine-gallium lamp 1-1.2m Exposure Energy: 160-180 mj/cm2 Resolution: 2% - 98% at 200lpi Ugra Reading: Recommended to use 13 step scale / three steps clear Run Length: 50,000-80,000 (Actual run length may vary according to press, ink and paper condition.) Recommended Developer: Ronsein developer or Fuji developer Protection Gum: Suitable to any PS plate protection gum Developing Temperature: 21-25 degree Celsius Developing Time: 25-35s Developer[...]

2018-12-15Szczegóły...

[Chiny]Offset Printing Plate

Thickness: 0.15-0.30mm Spectral Sensitivity: 3000W iodine-gallium lamp 1-1.2m Exposure Energy: 160-180 mj/cm2 Resolution: 2% - 98% at 200lpi Ugra Reading: Recommended to use 13 step scale / three steps clear Run Length: 50,000-80,000 (Actual run length may vary according to press, ink and paper condition.) Recommended Developer: Ronsein developer or Fuji developer Protection Gum: Suitable to any PS plate protection gum Developing Temperature: 21-25 degree Celsius Developing Time: 25-35s Developer[...]

2018-12-15Szczegóły...

[Chiny]Thermal Plate

Thickness: 0.15-0.30mm Spectral Sensitivity: 830nm Exposure Energy: 130-150 mj/cm2 Resolution: 1%-99% at 250lpi FM Capability: 20um Run Length: 100,000(Actual run length may vary according to press, ink and paper condition.) Recommend Developer: Ronsein developer or Kodak developer Protection Gum: Recommended to use 140G protection gum Developing Temperature: 22-24 degree Celsius Developing Time: 25-35s Replenishment Rate: 100ml/sqm Baking Preparation: Applied any suitable plate baking[...]

2018-12-15Szczegóły...

[Chiny]Digital Direct Plate

Thickness: 0.15-0.30mm Spectral Sensitivity: 830nm Exposure Energy: 130-150 mj/cm2 Resolution: 1%-99% at 250lpi FM Capability: 20um Run Length: 100,000(Actual run length may vary according to press, ink and paper condition.) Recommend Developer: Ronsein developer or Kodak developer Protection Gum: Recommended to use 140G protection gum Developing Temperature: 22-24 degree Celsius Developing Time: 25-35s Replenishment Rate: 100ml/sqm Baking Preparation: Applied any suitable plate baking[...]

2018-12-15Szczegóły...

[Chiny]UV Plate

Thickness: 0.15-0.30mm Sensitive Wavelength: 400-430nm Photosensitivity: 60-80 mj/cm2 Dot reproduction: 1%-99% at 200lpi (2400dpi) Micro-line reproduction: 6-10um Run Length: 50000-80000(Actual run length may vary according to press, ink and paper condition.) Recommend Developer: Ronsein developer or Fuji developer Developer Concentration: liquid to powder =1:4 (automatic);liquid to powder =1:6 (manual) Developing Temperature: 21-25 degree Celsius Developing Time: 25-35s Baking Temperature:[...]

2018-12-15Szczegóły...

[Chiny]Positive PS Printing Plate

KLP-SS is the best sold and cost effective plate of Konita with the high sensitivity , steady network and long run length. Konita's positive PS plate KLP-SS and KLP-A had been selected as OEM products for the Japanese company Konica and sold abroad in 2003,and win good feedbacks and an increasing numbers of orders. Konita has cooperated with RR Donnelley and Cron for years and enjoys great reputation both in China and other countries. Properties: 1) High sensitivity : High photosensitive[...]

2018-12-13Szczegóły...

[Chiny]VP-380 Solid ink roll coder

Adopt photoelectric mechanism technology, automatic temperature Control, Auto counting, adjustable print position Adopt solid ink roll, legible printing, fast dry, and color selectable, not easy to remove. With multi functional print wheel, maximum 5 lines, 15 characters have 2mm, 2.5mm, 3 mmtypes for your choice.Fit for printing on paper, plastic film and aluminum foil materials,such as cardboard,plastic bag,flat cartons and so on in high speed and high efficiency, up to 300 pcs per minute.[...]

2018-12-13Szczegóły...

[Chiny]Thermal CTP Plate

Thickness: 0.15-0.30mm Spectral Sensitivity: 830nm Exposure Energy: 130-150 mj/cm2 Resolution: 1%-99% at 250lpi FM Capability: 20um Run Length: 100,000(Actual run length may vary according to press, ink and paper condition.) Recommend Developer: Ronsein developer or Kodak developer Protection Gum: Recommended to use 140G protection gum Developing Temperature: 22-24 degree Celsius Developing Time: 25-35s Replenishment Rate: 100ml/sqm Baking Preparation: Applied any suitable plate baking[...]

2018-12-11Szczegóły...

[Chiny]CTP Plate

Thickness: 0.15-0.30mm Spectral Sensitivity: 830nm Exposure Energy: 130-150 mj/cm2 Resolution: 1%-99% at 250lpi FM Capability: 20um Run Length: 100,000(Actual run length may vary according to press, ink and paper condition.) Recommend Developer: Ronsein developer or Kodak developer Protection Gum: Recommended to use 140G protection gum Developing Temperature: 22-24 degree Celsius Developing Time: 25-35s Replenishment Rate: 100ml/sqm Baking Preparation: Applied any suitable plate baking[...]

2018-12-11Szczegóły...

[Chiny]UV-CTP Plate/CTCP Plate

Thickness: 0.15-0.30mm Sensitive Wavelength: 400-430nm Photosensitivity: 60-80 mj/cm2 Dot reproduction: 1%-99% at 200lpi (2400dpi) Micro-line reproduction: 6-10um Run Length: 50000-80000(Actual run length may vary according to press, ink and paper condition.) Recommend Developer: Ronsein developer or Fuji developer Developer Concentration: liquid to powder =1:4 (automatic);liquid to powder =1:6 (manual) Developing Temperature: 21-25 degree Celsius Developing Time: 25-35s Baking Temperature:[...]

2018-12-11Szczegóły...